Quel type de colorant à base de farine de chromite faut-il utiliser pour la fabrication de bouteilles en verre vert ?

Raw material: South‑African chromite ore powder (Glass‑Grade Chromite Flour). The mainstream industry grade: Cr₂O₃ ≥46%, 325 mesh (-325#).
 Standard Specifications (Commonly Adopted by Glass Plants)
Chemical Indexes (Glass‑coloring Grade)
ItemSpecification
Cr₂O₃≥46.0%
SiO₂≤1.0% (Excessive silica causes devitrification and spots)
CaO≤0.30% (CaO shall be strictly controlled)
P, S≤0.003% (Trace impurities to prevent bubble formation)
Cr/Fe Ratio1.55:1

Particle Size Selection

  • 325 mesh (45 μm, 98% passing) [Most Popular]: First‑choice for olive‑green beer bottles. It achieves complete melting without black spots or color mottling, delivering uniform and stable color.
  • 200 mesh: Used in some old production lines. Larger particles tend to trigger black spots, and this grade is gradually replaced by 325 mesh.
  • 400‑600 mesh: For high‑grade emerald‑green glass bottles with better dispersion at higher cost.